NIBIOs ansatte publiserer flere hundre vitenskapelige artikler og forskningsrapporter hvert år. Her finner du referanser og lenker til publikasjoner og andre forsknings- og formidlingsaktiviteter. Samlingen oppdateres løpende med både nytt og historisk materiale. For mer informasjon om NIBIOs publikasjoner, besøk NIBIOs bibliotek.

2005

Sammendrag

In this study modified wood samples were tested according to the extended standardised test procedures of ENV 807 (3 types of soils). A Round Robin test was carried out at two laboratories: Swedish National Testing and Research Institute and Norwegian Forest Research Institute.The different soil types used were conifer forest soil (pH 4.6), soil from the Simlngsdalen test field (pH 5.2) and garden compost soil (pH 7.4). The wood modifications used were furfurylation (Visorwood), acetylation and heat treatment (Thermowood). Other materials tested were linseed oil impregnated pine, reference preservative (CC and CCA) treated pine and Robinia psuedoaccacia heartwood.A dynamic MOE (MOEdyn) test device based on measurement of ultrasonic pulse propagation was used for non-destructive decay strength evaluation during the incubation period. The MOE values were correlated to measured decay mass loss of the test specimens after different periods of exposure to the soils. Type of fungal attack was also evaluated using light microscopy.Results from preliminary studies indicate that ultrasound seems to be an excellent tool for evaluation of early brown rot decay. It also seems to be feasible for detecting white rot. However it does not seem to be very accurate in evaluating early stages of soft rot decay.

Sammendrag

Wood samples treated with ammonium copper quat (ACQ 1900 and ACQ 2200), chromated copper arsenate (CCA), Tanalith E 3491 and Wolmanit CX-8 have been studied in accelerated weathering experiments. The weathering experiment was performed by cycles of 2 h UV-light irradiation followed by water spray for 18 min. The changes on the surface of the weathered samples were characterized by roughness and color measurements on the samples with 0, 200, 400 and 600 h of total weathering.The objective of this study was to investigate the changes created by weathering on impregnated wood with several different wood preservatives. This study was performed on the accelerated weathering test cycle, using UVirradiation and water spray in order to simulate natural weathering. Surface roughness and color measurement was used to investigate the changes after several intervals (0200400600 h) in artificial weathering of treated and untreated wood.

Sammendrag

Fungi cause serious problems in wood utilization, and environmentally benign wood protection is required as an alternative to traditional chemicals. Chitosan has shown promising antimicrobial properties against several microorganisms. In this study, we present the characterization of and antifungal properties of a commercial chitosan formulation developed for impregnation of wood.A broad range of chemical and mycological methods were used to evaluate the uptake, fixation, and antifungal properties of chitosan for wood preservation. The results show that the higher the uptake of chitosan the lower the relative recovery of chitosan in wood after leaching, and the higher the molecular weight of chitosan the higher the recovery.Chitosan with high molecular weight proved to be more efficient against decay fungi than chitosan with low molecular weight. The fungi tested on chitosan-amended nutrient agar medium were totally inhibited at 1% (w/v) concentration.In decay studies using small wood blocks, 4.8% (w/v) chitosan concentration gave the best protection against brown rot fungi.

Sammendrag

During a period of 2 years and 3 months (1 January 2001 - 20 March 2003) Mycoteam had 3161 consultations in buildings in southern Norway, 1428 revealing damage from decay fungi. One consultation often revealed several occurrences of fungi, and the total number of occurrences of decay fungi was 3434. Thirty-five different species/genera/groups of decay fungi were recorded. During this period brown rot was more frequent (77.4 %) than soft rot (19.2 %) and white rot (3.4 %). Coniophora puteana (16.3 %) and Serpula lacrymans (16 %) were the most frequently identified species. Different species of the genus Antrodia were recorded in 18.4 % of the occurrences, while the group Corticiaceae accounted for 5.7 % and soft rot for 15.8 %. Investigations of damaged structural parts of buildings showed that decay fungi were most common in walls (18.3 %). Floor damage accounted for 13.4 % of the damaged structures and roofs for 8.8 %. Nearly all species and groups of the investigated fungi were most common indoors. Gloeophyllum sepiarium on the other hand was most common outdoors, and Dacrymyces stillatus was exclusively found outdoors. The Norwegian data were compared with published time series data from Denmark (1946-66, 1966-71, 1974-75, 1982) and Finland (1978-84, 1985-88). S. lacrymans and C. puteana were the most frequent species in these datasets too. Antrodia spp. were also common in the Finnish reports, but barely recorded (as identified species) in Denmark. In both the Danish and the Finnish data, damage to floors is the most frequently recorded structural damage in buildings.

Sammendrag

This paper describes the use of quantitative real-time PCR for monitoring colonization of birch wood (Betula pubescens) by the white-rot fungus Trametes versicolor in an EN113 decay experiment. The wood samples were harvested after 4, 8, 12, 16 and 20 weeks of incubation.The mass loss was in the range of 440%. Chitin and ergosterol assays were conducted for comparison. Second-order polynomial fits of the mass loss of decayed wood versus chitin, ergosterol and DNA gave correlations (r2) of 0.87, 0.61 and 0.84, respectively. Compared to the other two assays employed, real-time PCR data correlated best with the relative mass loss of decayed samples 48 weeks after inoculation, while the saturation and decline of DNA-based estimates for fungal colonization 1620 weeks after inoculation indicated that the DNA assay is not suited for quantification purposes in the late stages of decay.The impact of conversion factors, extraction efficiency, inhibitory compounds and background levels in relation to the three detection assays used is discussed.

2004

Sammendrag

A method for determination of the climate gases CH4, CO2 and N2O in air samples and soil atmosphere was developed using GC-MS. The method uses straightforward gas chromatography (separation of the gases) with a mass spectrometric detector in single ion mode (specific determination).The gases were determined with high sensitivity and high sample throughput (18 samples h1). The LOD (3) for the gases were 0.10 L L1 for CH4, 20 L L1 for CO2 and 0.02 L L1 for N2O. The linear range (R2 = 0.999) was up to 500 L L1 for CH4, 4000 L L1 for CO2 and 80 L L1 for N2O. The samples were collected in 10 mL vials and a 5 L aliquot was injected on column.The method was tested against certified gas references, the analytical data gave an accuracy within 5% and a precision of 3%. The presence of 10% by volume of C2H2 (often used experimentally to prevent N2 formation from N2O) did not interfere with detection for the targeted trace gases.

Sammendrag

A home designed diffusion chamber was used during the isolation of fluoride from plant material. The chamber contained two beakers, one for the sample (milled plant material) and the other for the trapping solution (0.1M NaOH). Hexamethyldisiloxane (HMDS) in 3.5M perchloric acid was added into the sample beaker through a septum, after the chamber was closed.Fluoride in the sample reacts with HMDS and forms the volatile trimethylfluorosilane (TMFS), which is trapped and hydrolyzed to fluoride. The diffusion time was 2h and 20 samples were handled at the same time. The fluoride concentration was determined by a flow injection analysis (FIA) system using an ion selective electrode (about 50 samples/hour).The results by acid extraction were compared to the results obtained after an ashing/alkaline fusion. Both a certified sample of timothy grass (NIST 2695, high level) and more typical vegetation from forest were analyzed. For the timothy grass, the recovery increased from 48 to 84% when ashing/alkali fusion was used before the diffusion. However, higher recovery was not obtained by using ashing/alkaline fusion for the determination of fluoride in natural vegetation from forest. Acid extraction in combination with addition of HMDS was sufficient as pretreatment in these types of plant materials.The method was routinely used for the determination of fluoride both in research and forest monitoring.

Sammendrag

In this study modified linseed oils, rape oil and three waxes were screened on their efficacy as wood protecting agents. By testing all products when impregnated with high retentions in Scots Pine sapwood on water repellence qualities, additionally an accelerated weathering test, drying quality, accelerated brown rot and blue stain test, an indication is formed of the capability of these products as wood protecting treatments. All oil and wax treatments significantly improve the water repellency of untreated wood. In weathering resistance, maleinised and polymerised linseed oil showed the best results in improving untreated pine sapwood dimensional stability thus reducing crack formation and decolourization by UV-light. In accelerated brown rot and blue stain tests boiled linseed oil significantly reduced degradation and staining. In addition, maleinised linseed oil and a mixture of modified linseed- and mineral oil are very well performing in the blue stain test. Overall most promising products are the maleinised oils and boiled linseed oil. The maleinised oils have good potentials in long lasting water repellency, showed some fungal growth prevention, are colour stable in weathering tests and create a dimensional stable wood product. Boiled linseed oil is not exceptionally good as a water repellent, but the good drying qualities together with easy handling makes this oil a promising product.