NIBIOs ansatte publiserer flere hundre vitenskapelige artikler og forskningsrapporter hvert år. Her finner du referanser og lenker til publikasjoner og andre forsknings- og formidlingsaktiviteter. Samlingen oppdateres løpende med både nytt og historisk materiale. For mer informasjon om NIBIOs publikasjoner, besøk NIBIOs bibliotek.
2011
Sammendrag
Det er ikke registrert sammendrag
Sammendrag
Wood exhibits a highly anisotropic mechanical behavior due to its heterogeneous microscopic structure and composition. Its microstructure is organized in a strictly hierarchical manner from a length scale of some nanometers, where the elementary constituents cellulose, hemicelluloses, lignin, and extractives are found, up to a length scale of some millimeters, where growth rings composed of earlywood and latewood are observed. To resolve the microscale origin of the mechanical response of the macro-homogeneous but micro-heterogeneous material wood, micromechanical modeling techniques were applied. They allow for prediction of clear wood stiffness (Hofstetter et al. 2005,2007, Bader et al. 2010a,b) from microstructural characteristics. Fungal decay causes changes in the wood microstructure, expressed by decomposition or degradation of its components (Côté 1965, Schwarze 2007). Consequently, macroscopic mechanical properties are decreasing (see e.g. Wilcox 1978). Thus, in the same manner as for clear wood, consideration of alterations of wood in a micromechanical model allows predicting changes in the macroscopic mechanical properties. This contribution covers results from an extensive experimental program, where changes in chemophysical properties and corresponding changes in the mechanical behavior were investigated. For this purpose, pine (Pinus sylvestris) sapwood samples were measured in the reference condition, as well as degraded by brown rot (G. loeophyllum trabeum) or white rot (Trametes. versicolor). Stiffness properties of the unaffected and the degraded material were not only measured in uniaxial tension tests in the longitudinal direction, but also in the three principal material directions by means of ultrasonic testing. The experiments revealed transversal stiffness properties to be much more sensitive to degradation than longitudinal stiffness properties. This is due to the degradation of the polymer matrix between the cellulose fibers, which has a strong effect on the transversal stiffness. On the contrary, longitudinal stiffness is mainly governed by cellulose, which is more stable with respect to degradation by fungi. Consequently, transversal stiffness properties or ratios of normal stiffness tensor components may constitute suitable durability indicators. Subsequently, simple micromechanical models, as well as a multiscale micromechanical model for wood stiffness, were applied for verification of hypotheses on degradation mechanisms and model validation.
Forfattere
Trygve D. Kjellsen Igor A. Yakovlev Carl Gunnar Fossdal Richard StrimbeckSammendrag
Siberian spruce (Picea obovata) grows in the coldest forested environments on Earth, with average temperatures in midwinter months below -40 C and record lows below 60 C. Fully acclimated needles of this species survive immersion in liquid nitrogen at -196 C provided they are first cooled to an intermediate temperature of around -30 C. To investigate the role of dehydrins in extreme frost tolerance, we monitored frost tolerance, relative dehydrin concentration, and relative changes in dehydrin transcript levels in P. obovata needles over a full acclimation-deacclimation cycle.
Sammendrag
Det er ikke registrert sammendrag
Forfattere
Bernt HoelSammendrag
Det er ikke registrert sammendrag
Forfattere
Bernt Hoel Hans TandsætherSammendrag
Det er ikke registrert sammendrag
Forfattere
Hanna Marika Silvennoinen Annelene Pengerud Christina Biasi Peter DörschSammendrag
Det er ikke registrert sammendrag
Sammendrag
Det er ikke registrert sammendrag
Sammendrag
Luserne (Medicago sativa L.) er ein fôrvekst med stort avlingspotensial, og tilpassa sortar greier seg godt i låglandet i Sør-Norge. Luserne krev god jordstruktur og høg pH i jorda for å trivast, og frøet må smittast med rett type bakteriekultur før såing. Nitrogenfikseringa kan bli høg der arten trivst. Fôrverdien er høgast på ungt stadium, og energiverdien går raskt ned med aukande stengelutvikling. Proteinverdien er generelt høg. Norsk foredlingsmateriale er meir hardført enn utanlandsk plantemateriale, og nye foredlingslinjer (LøLu9822, LøLu9823) har gjort det betre i forsøk enn sorten "Live". Linja LøLu9821 ser ut til å vera mest hardfør. I forskingsrådprosjektet "Engbelgvekstar - dyrking - klima" blir ulike lusernelinjer prøvt i utkanten av mulig dyrkingsområde, og dyrkingsteknikk til luserne blir nærmare undersøkt på Bioforsk-stasjonane Apelsvoll, Løken og Tjøtta.
Forfattere
Petter MarumSammendrag
Engvekstene dekker det største arealet av dyrket mark her i landet. Det er derfor viktig med sorter som på en best mulig grad utnytter dyrkingsforholdene på stedet. Hvert år etableres det omlag 700.000 daa ny eng som blir høstet over flere år. I følge Statistisk sentralbyrå ble det høstet 2 698 000 000 kg høy (omregnet til kg høy) i 2009. En liten avlingsøkning eller kvalitetsøkning som skyldes sortene vil derfor ha stor effekt. 1 % økning tilsvarer en mer avling på 26 980 000 kg. Innlegg under Bioforsk-konferansen 2011. Last ned pdf av artikkel og presentasjon under "Les mer" til høyre.